We have performed the type of test you describe. Please feel free to contact me if we can be of service.
As you suggest, you do get a large number of data points. In past programs we've wound up with
approximately one reading per second per channel. The computer can automatically flag predefined alarms.
We then import all the data into a spreadsheet, identify maximum and minimum resistances and graph the
data.
Chan, Marcelo wrote:
> I would like to know if it is possible these days to conduct reliability tests
> on daisy chain components and monitor < 2 Ohms resistance change rather than
> just continuity... I understand that I could utilize the four probe resistance
> approach, but I would like to monitor about 100 devices simultaneously...I am
> looking manageable approaches for upgrading our current continuity approach....
> Also, how do people overcome the data logging of intermittent failures without
> causing a tremendous amount of data.... on one hand, we want to capture an open
> during temperature cycling, but not log the same device over and over again in a
> span of 1 second....
>
> Thanks,
>
> Marcelo
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
--
John Moylan
President
Delsen Testing Laboratories, Inc.
1024 Grand Central Ave.
Glendale, CA 91201
Phone: 818 247 4106
FAX 818 247 4537
email: [log in to unmask]
URL: http://www.primenet.com/~delsen/
Delsen Testing Laboratories, Inc. is an independent testing
laboratory primarily engaged testing advanced materials.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|