TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 15 Jan 2004 09:53:07 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset="us-ascii"
Subject:
From:
Dave Hillman <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
Hi Don! Here's a quick answer - if the Sn/Pb component finish is not
sufficiently thick you will run the risk of degrading the solderability -
the higher the bake temperature the quicker/greater the degradation. Good
Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




                      Donald Vischulis
                      <dvischulis@earth        To:       [log in to unmask]
                      link.net>                cc:
                      Sent by: TechNet         Subject:  [TN] MSD Question
                      <[log in to unmask]>


                      01/14/2004 08:26
                      PM
                      Please respond to
                      Donald Vischulis






Just a quick question:  What is your opinion of a MSD control procedure the
requires baking tin/lead terminated (coated) components every 7 days?

Don Vischulis

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2