TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Fri, 30 Nov 2007 16:59:29 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (286 lines)
HO HO or do I mean OH OH





Regards 

Mike 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Thursday, November 29, 2007 10:38 PM
To: [log in to unmask]
Subject: Re: [TN] SN100C process

Yes you will, in fact you could probably write a brown paper on the
subject..............8-)

Your spolling is attricious...

John

 
 
John Burke
 
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Thursday, November 29, 2007 2:26 PM
To: [log in to unmask]
Subject: Re: [TN] SN100C process

Whoops, yes did my sums wrong, the key temperature is the one measured in
the wave, but if your machine cant actually melt the pot contents adequately
then you are likely to have issues arsing from poor alloy homogeneity.





Regards 

Mike Fenner
Indium Corporation 

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com 

---------------------

Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence)
77-97 Harpur Street, Bedford , UK
Registered number: fc16473


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Thursday, November 29, 2007 3:19 PM
To: [log in to unmask]
Subject: Re: [TN] SN100C process

Mike,

Thanks for the insight. What worries me is that 540F is actually 280C. I
didn't go there yet, but I am at 274C (525F) and still see the solder
freezing at the corners of the pot. Although this must be a machine issue,
did not get much help from the manufacturer.

I've got your point regarding VOC free fluxes.

Thanks,

Ioan

-----Message d'origine-----
De : Mike Fenner [mailto:[log in to unmask]] Envoyé : 29 novembre 2007 09:47
À : 'TechNet E-Mail Forum'; Ioan Tempea Objet : RE: [TN] SN100C process

While we wait for Ronnie......

540F is about 250something C, that's about in the 'normal' range. Don't
forget the SN100C is a tin/copper not a SAC and so has a higher MP/operating
range. 

For LF wave soldering you probably need to have a little higher solids than
for leaded, and some VOC formulations are definitely more suited to lead
free than IPA based materials. This is all down to the properties of high SN
content of lead free alloys and their associated temperatures as a whole
rather than specific differences between them.

You should be able to solder satisfactorily without nitrogen as a soldering
aid, but do have nitrogen as a dross limiter.

Specific process parameters will depend on your specific alloy ,machine,
flux and board type. You will probably be better to have those conversations
individually off line or get ideas from other user experiences.

Overall there is no intrinsic reason why you should not be able to wave
solder lead free with very low defect levels, board/design/components are
still the ultimate limiting factors in this process.




Regards 

Mike Fenner
Indium Corporation 

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com 

---------------------

Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence)
77-97 Harpur Street, Bedford , UK
Registered number: fc16473


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Wednesday, November 28, 2007 3:55 PM
To: [log in to unmask]
Subject: [TN] SN100C process

Dear Technos,

 

I have moved to this new company and here we're running SN100C in wave, as
opposed to the SAC305 I used to have before. So I have to start all over
defining the baseline process parameters.

 

Besides frequent shorts and solder not going all the way to the top, we have
an issue with solder freezing at the corners of the solder pot. To overcome
this "chilly" issue, we were suggested to run the pot at 540F!

 

So I would like to know where you are with the SN100C:

*          What pot temperature

*          What conveyor speed range

*          What flux (special formulation for the alloy or regular,
solids content, water or alcohol based, etc)

*          Nitrogen or not

*          Other particular points of interest

 

Of course an insight regarding the attainable defect free yields would also
be appreciated.

 

Thank you,

 

Ioan


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient, please contact the
sender by return and delete the material from any computer. Any review,
retransmission, dissemination, or other use of, or taking of any action in
reliance upon this information by persons or entities other than the
intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. Indium Corporation does
not accept responsibility for changes made to this email after is was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***"

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient, please contact the
sender by return and delete the material from any computer. Any review,
retransmission, dissemination, or other use of, or taking of any action in
reliance upon this information by persons or entities other than the
intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. Indium Corporation does
not accept responsibility for changes made to this email after is was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***"

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***"

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2