I have used a Soft-Beam system for some limited rework as well as a medium
quantity production, in-line operation. The key factors for using this
system included temperature sensitivity for surrounding components, high
thermal mass in the solder joints that needed selective soldering, components
that could be easily fixtured after insertion so that they did not fall out
when the board is inverted for the Soft-Beam operation.
In general the Soft-Beam performed fairly well. The biggest hassle was the
calibration of the shutter cycle as the bulb aged. Since that bulb reduces
in output over time, a calibration routine is required to ensure the process
remains stable. For our process control limits, running the system 24/7,
that meant running calibration weekly on a new bulb, 2x weekly in mid bulb
life and 3-4x weekly toward the end of bulb life.
Solder joint quality looked good in both visual inspection and
cross-section. The ability to preheat each joint before applying solder
helped. Of course that also adds to cycle time.
Jon Moore
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|