TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Date:
Fri, 12 Jun 2009 17:06:24 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, fabrice pires <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
fabrice pires <[log in to unmask]>
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
In-Reply-To:
Organization:
Thales-EPM
MIME-Version:
1.0
Parts/Attachments:
text/plain (60 lines)
It make me think about creep corrosion phenomena. Is there any sulfur in 
the residues?
Just an idea.


Karen Tellefsen a écrit :
> One of our technical service engineers asked me about a strange migration
> phenomenon one of our customers observed under passives and QFN's that have
> been soldered with one of our no-clean SAC305 solder pastes. I've attached
> an X-ray picture of a QFN exhibiting this strange failure, but I don't know
> how it can be posted so you can look at it.. Further analysis after
> removing the component showed that the shadows in the X-ray picture is
> caused by a black material containing tin. The boards were conditioned 85°C
> 85%RH  for 500 hr, but no voltage was applied.  This phenomenon was not
> observed under QFPs (not surprising), and seems to be independent of reflow
> profile used.  Additionally, the customer has not seen anything like this
> with tin lead solder paste, however, the tin-lead solder pastes would have
> a different fluxes.   The tin "migration" is coming from both adjacent
> solder joints, and there is no voltage applied, so it seems to be a
> corrosion problem.  Certainly QFN and big passives are good at trapping and
> retaining water in the flux residue underneath them.
>
> I've never seen anything like this; has anyone else out in TechNet land
> seen this or have any ideas what caused this?
>
> Thanks
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
> (See attached file: Strange tin migration.JPG)
>
>
> Enthone GmbH  Geschäftsführer: Knut Balzer, Luc de Croo, Jürgen Dietrich  Amtsgericht Düsseldorf  HRB 45276
> USt-Id-Nr. DE 811 205 946 
>
>
> This communication is for use by the intended recipient and contains information that may be privileged, confidential or copyrighted under applicable law.  If you are not the intended recipient, you are hereby formally notified that any use, copying or distribution of this e-mail, in whole or in part, is strictly prohibited.  Please notify the sender by return e-mail and delete this e-mail from your system.  Unless explicitly and conspicuously designated as "E-Contract Intended", this e-mail does not constitute a contract offer, a contract amendment, or an acceptance of a contract offer.  This e-mail does not constitute a consent to the use of sender's contact information for direct marketing purposes or for transfers of data to third parties.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>   

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2