Tin has two potential problems.

A shelf life problem, unaffected by the atmosphere it is stored in, where
spontaneous alloying occurs as the Copper and Tin form an "intermetallic".
It is my understanding that when all of the Tin becomes part of the
intermetallic layer, the surface is no longer solderable.

The other issue is oxidation.  Tin Oxide is particularly difficult to solder
over, and if it is thick enough, not even the most aggressive flux will work.
 This issue is strongly affected by the atmosphere the board is stored in.

Both problems are accelerated by heat.

I hope this helps.

Rudy Sedlak
RD Chemical Company

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2