Susan,
Thanks for the feedback.
Since the inner layers must be attached we would have to cross-section to see
if that were the condition, which would destroy the board anyway.
We are sure of the HASL stress as the cause first, by visual and later by cross-
section. It involved only thick (.200") boards. We solved the problem by baking
the boards for 4-8 hrs @ 300F, although we don't really know if the pullaway
was due to trapped moisture or the "shock" of HASL.
Joe
Quoting [log in to unmask]:
> Joe
> I have seen many microsections in years passed where the plating was
> stuck to
> the inner layers only and none to the laminate. Inner layers must be
> attached. Military specs still have a resin recession requirement "as
> received". IPC specs evaluate after stress and therefore have dropped
> the
> consideration that resin recession is a defect.
>
> The theory being if there is no requirement after stress, then why have
> a
> limit before?
>
> Inner layers must be attached.
>
> How do you know the hole wall "explodes" or "delaminates" after HASL?
> Is
> this by microsection or visual assessment?
>
> Susan
>
Joseph Spicuzza
Quality Assurance Supervisor
Advanced Interconnect Products Division
Compunetics, Inc.
ph: 412 858-6166
fax 412 373-8060
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|