TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 4 Sep 2008 14:40:59 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
From:
Phil Nutting <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (86 lines)
Second try at sending, E-mail server said it didn't go out.


Graham,

We had a similar issue with large gauge wires.  We found the sweet setup in Esico-Triton Resistance soldering equipment. http://www.esicotriton.com/resistance/

Do you think 1000 Watts would be enough?  We have one and it is amazing.  Huge pieces are at soldering temperatures in a matter of seconds! Yes seconds... about 2 or 3 seconds.  You can make parts cherry red faster with this than with a torch and the heat is much better controlled with regard to placement of heat.  A torch heats up a huge area and this gadget heats up a small spot via contact of graphite tips.  This is where I would insert the Tim Allen grunt of very cool approval.

For years we had use a much smaller version that wasn't up to the big lug task, but they worked great for small items.

You will not regret buying one of these if you have to solder 0 AWG wire in big copper lugs on a regular basis.  Your process time will be reduced by using this machine.

You can buy direct from Esico-Triton or through several distributors such as Newark, Stanley Supply, Techni-tool and Mouser.

Phil Nutting

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Thursday, September 04, 2008 12:53 PM
To: [log in to unmask]
Subject: Re: [TN] Wire Harness question - soldering 0 AWG wire?

Hi Graham,

Like Jerry I've never done it but I remember seeing someone solder very
large wire into a very large terminal with a small torch. I don't recall
anything more than that but I might lead you in a direction (kicking and
screaming :-)

KennyB

-----Original Message-----
From: Jerry Dengler [mailto:[log in to unmask]]
Sent: Thursday, September 04, 2008 9:49 AM
To: [log in to unmask]
Subject: Re: [TN] Wire Harness question - soldering 0 AWG wire?

Hi Graham,

I've never done this myself but watched it being done at a customers
site.  The had to make a holder for the connector that had a temperature
controlled heater in it.  I believe they used a 50 watt iron.

Regards,

Jerry Dengler
Production Manager
Pergamon Corporation
PH:  610-239-0721
Fax: 610-239-0720


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Thursday, September 04, 2008 12:35 PM
To: [log in to unmask]
Subject: [TN] Wire Harness question - soldering 0 AWG wire?

Hello TechNet
I've been dragged (kicking and screaming) out of my comfort zone, and am
looking at a wire harness.  I've got some 0 awg wire to solder into a
connector.  We haven't tried it, but I really doubt that my Metcal
MX-500 system is up to this task.  Do any of you have experience with
this, and if so can you recommend equipment or technique?

regards,

Graham Collins
Halifax Production Engineering
(902) 873-2000 ext. 6215



Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2