TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 9 Jun 2006 10:56:54 -0700
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Lee <[log in to unmask]>
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Peter Lee <[log in to unmask]>
Content-disposition:
inline
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (19 lines)
Does anyone have recommendation on a process to remove self-clinching PEM nut from the board? An incorrect 4-40 size and 1/4" long nut was mistakenly installed and needs to be removed and replaced with a similar but shorter nut.

Would I lose much of the clinching strength by re-using the hole? Is there any work-around to reinforce the hole to achieve the similar pull strength as before?

Any suggestion is appreciated.

Rgds,
Peter

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2