Phil,
Stewart-McDonald makes a conductive shielding paint used for guitar
cavities that might fill the bill. I don't know what the conductive media is
though, could be carbon or copper. Or there is CuPro, which is copper
loaded. Neither one are cheap though....
http://www.stewmac.com/shop/Electronics,_pickups/Supplies:_Shielding/Conduct
ive_Shielding_Paint.html
http://www.lessemf.com/292.html
Mike McMonagle
Quality Engineer
OYO Geospace
7007 Pinemont Drive
Houston, TX 77040
713-986-8650
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Thursday, December 01, 2005 6:53 AM
To: [log in to unmask]
Subject: Re: [TN] Anti static sprays
Hmmmm... This is good information, but it is not relative to our
problem.
We have a high voltage generator in a molded plastic flame retardant
enclosure. We are finding that with the material presently used there
appears to be static charging going on which is causing instability and
arcing in the unit.
Certainly changing the material on the enclosure is probably the best
long term solution. The question is how can we improve the inventory we
have on hand so it is less prone to static charging. It is not
practical to recoat the unit regularly. I need to coat it once and have
it work for a very long time.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Wednesday, November 30, 2005 6:02 PM
To: [log in to unmask]
Subject: Re: [TN] Anti static sprays
Best place to apply an anti-stat is always last step in process.
Rudy Sedlak
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
Yahoo! Music Unlimited - Access over 1 million songs. Try it free.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|