TECHNET Archives

May 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Sun, 1 May 2011 20:05:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (30 lines)
Local water supplies vary greatly.
One location limed the water to lower its ph level to 8 to keep the lead out
of the drinking water.
Most of the water in the area was 5.0 to 6.5 ph.
Some areas have water so hard the calcium deposits in a cleaner would shut
it down in a few months.
I would use New York City water for a final rinse, there are few areas with
water that good.
Analyse the water and determine what is required to reach your cleanliness
requirements.

That 20M water drops to under a Meg as soon as it is in contact with the
air.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2