TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 8 Nov 2007 15:18:59 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Hi Eric,
Things are a little more complex than that, I am afraid.
I would suggest you obtain my White Paper "Recommendations for PCB FAB Notes 
and Specifications in Printed Circuit Board Drawings for SnPb and Lead-Free 
Soldering Assemblies, the Qualification of PCB Shops and Activities to Assure 
Continued Quality." It is to my knowledge the only pretty comprehensive [cannot 
be totally comprehensive becaus ethis is a very fast mocing situation] source 
dealing with all the issues of PCB specifications. 
Please go to my website for details.

Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com



**************************************
 See what's new at http://www.aol.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2