TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Date:
Thu, 4 Apr 2002 07:10:56 EST
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (40 lines)
Hi Wee Mei,
To your questions:
>Q1 : Single-sided board reliability.
>- in the usual fabrication process, single sided board only have pads on
>one side and the holes are not plated-through. What is the chances that
>the component will fly off or pads lifted during vibration test?
A: It will depend on the severity of the vib test and the weight of the
component. Single-sided boards should be regarded as Class 1.
>- if everything remain but the hole wall is plated, will the solder
>joint now be more robust to withstand vibration or the component will
>stay put or pads will not be lifted?
A: This will certainly be more robust.
>Q2 : warpage
>- I noticed that warpage indicated in the IPC standard usually are
>confined to boards that are 4 sided. For my board, flatness is a must
>but the board is of odd shape or irregular shape. How do I perform the
>warp test and acceptance?
A: Put the boards on a flat surface; if they are warped they will rock. The
amount of rocking is a measure of the warp severity--you have to figure out
what is good enough.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2