CLTE is a PTFE based material. CTE X 10 PPM, Y 12 PPM, and Z 40 PPM.
Tg????? This is a thermoplastic. Soft Stuff always unless you freeze
it. Ceramic Filled/Woven PTFE. I guess the Tg could be somewhere
around 75'C, but that's really not a valid question.
Groovy
______________________________ Reply Separator _________________________________
Subject: FAB: Arlon
Author: [log in to unmask] at SMTPLINK-HADCO
Date: 11/13/96 3:48 PM
Anybody familiar with the board laminate material Arlon-CLTE ? What
are the associated properties such as Tg(degC) ? CTE ppm/degC for X &
Y and the Z axis ?
D.Drake
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|