Hi Steve,
Vague but I'm game.
Which conformal coating? (To give me some idea of volatiles - an example
liquid Humiseal 1B31 is only 38% acrylic polymer, the rest is Toluene and
MEK)
Final (Dry) thickness of Conformal Coating?
Method of application: Dip, Spray, Needle
Means of application: Manual or Automatic (And yes I wish I had an
automatic coater.)
Amount you will accidentally spill right before a tour comes through . . .
:->
Don't forget any masking material, thinner and stripper (in case you need to
do rework).
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials (Process & Manufacturing) Engineer
Warner Robins Air Logistics Center
Avionics Production Division
Manufacturing Branch
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
-----Original Message-----
From: Steve Collins [mailto:[log in to unmask]]
Sent: Friday, July 07, 2000 3:40 PM
To: [log in to unmask]
Subject: [TN] Conformal Coat question
Forgive me if this question is sort of vague but the answer is required so
we can complete a BOM requirement.
How much liquid silicone (conformal coating) (oz) is required to cover 1 sq
in on a PCB.
Steve
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|