TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bloomquist, Ken" <[log in to unmask]>
Date:
Wed, 27 Oct 2004 16:20:18 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Janoch Jiří, Ing." <[log in to unmask]>
Subject:
From:
"Janoch Jiří, Ing." <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-2"
MIME-Version:
1.0
Parts/Attachments:
text/plain (55 lines)
Hi,
gold plating is common PCB finish. Embrittlement depends on gold
thickness. Simply, the more Au the more embrittlement.

Regards
J. Janoch, TSE

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Wednesday, October 27, 2004 3:53 PM
To: [log in to unmask]
Subject: [TN] Gold Board

Good morning TechNetters (at least here on the left coast),

We have a small assembly that requires a couple of pads to be gold
plated. We would like to gold plate the entire board but we're concerned
about gold embrittlement when we solder the components in. The board is
completely through hole and will be both wave soldered and hand
soldered.

Do you think we have any concerns? Oh by the way this is a class 3
assembly.

Thanks,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2