Hi Cathy! You may also want to search using the term "induction soldering".
There is a very good explanation of the subject in the AWS Soldering
Handbook (ISBN # 0-87171-618-6, author Paul Vianco), pages 406-418,
paragraph 6.4.3.5. The ASM Metals Handbook, Vol. 6, "Welding, Brazing, and
Soldering" has information on induction joining also. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Cathy Killen <[log in to unmask]>@ipc.org> on 09/05/2002 10:28:50 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Cathy Killen <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Eddy Current Soldering
I've searched everywhere for info on eddy current soldering, but can't find
anything. All info covers different topics of eddy currents but not
soldering. Can anyone help?
Cathy Killen
Training Instructor
The information contained in the E-mail is confidential. It is intended
only
for the stated addressee(s) and access to it by any other person is
unauthorised.
The views expressed in this E-mail are those of the author, and do not
represent the views of Smtek Europe, its associates or subsidiaries, unless
otherwise expressly indicated.
Please note: It is your responsibility to scan this E-mail for viruses.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|