TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Wed, 24 Nov 1999 14:03:29 +1100
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Well, Geoff, below 's your answer . If you'd need more details,
let us know .

Thanks Rudy ; boiling in lime sounds top application to me .
Nice no residue method indeed

paul

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, 24 November 1999 12:57
To: [log in to unmask]
Subject: Re: [TN] Ammoniacal Etchant


Thanks for the compliment, this will be fun.

To be specific, to "neutralize" usually means to adjust pH to make it legal,

or non-harmful.  The pH of spent etchant is usually between 8.0 and 9.0,
making it perfectly legal in even the US.

The problem is the HUGE contained metal content, that is heavily chelated to

keep it in solution.

To cut to the chase, you do not want to try to do remove this metal
yourself.
 Yes, you can do it, but, you do not want to, unless you use the Sigma-Mecer

system, which is very costly, unless you are large enough to amortize the
cost over a very large volume of etchant per day.  (I figure you do not want

to consider a Sigma-Mecer system unless you generate 55 gallons, around 200
liters, per day, but that is a guess).

Otherwise to get rid of the Copper, you either have to use expensive
precipitant, or dangerous Sulfides, and filter filter filter filter
filter...and wind up with vast amount of hazardous sludge.

Or, you can boil off the ammonia by adding caustic...no no no, just
kidding....

Don't do it yourself, unless you use the Sigma-Mecer system, it is a
nightmare, even for the folks who are in the reclaim business, they earn
their money.  You really do not want to consider this on a small scale.

What I would suggest, as an alternate, is to consider trying to make PCB's
differently, using Cupric, plus panel plate, plus tent and etch...the Cupric

is a helluva lot easier to deal with, and often you can find somebody who
wants to buy spent etchant from you to use for the contained copper salts.

Best,

Rudy Sedlak
RD Chemical Company

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2