Good Morning.
The advice from Kim is very good. This is commonly done, but there are a
bunch of items to consider.
1) Is the connector designed / not designed to do so? Certain connector
mfr's will claim so, most will not. Only those with military application
customers have any knowledge of it, and some have way more commercial
customers so it is not something they are willing to invest into.
It's been a while since I dealt with this, but to my recollection:
MIL-A-28870 assemblies using MIL-C-28859 contacts (NAFI) or EIA-???(UHD)
contacts will pierce AR, UR, and even XY coatings. IEH has a small line of
connectors that will as well. DIN 41612 and 2mm HM connectors will pierce
UR coating as well (although Harting and ERNI will not claim they do), but
not XY. Airborn connectors will NOT. At my last employer we kept a list of
connectors and mfr's we had used with success, but I no longer have it.
If not specifically designed to do so by the mfr, all is not lost - you can
run your own trials. Perform microsections to observe PTH integrity after
insertion. Check for electrical opens.
2) If so, what coating types (AR, UR, XY) and at what thicknesses?
3) What PCB parameters are required: drill size, plating thickness, FHS?
Hope that helps,
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, October 10, 2007 9:40 AM
To: [log in to unmask]
Subject: [TN] Installing Press-fit Connectors AFTER Conformal Coating?
Good Morning All!
We're about to build some assemblies for a customer that wants us to install
press-fit connectors after conformal coating. BTW, it's going to be an
acrylic coating.
This is something new for me. Is this pretty common? Is there anything I
should be careful of when doing this?
Thanks!
Steve Gregory
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|