Dear Jens,
As we produce PTFE PCBs, I can give you some answers:
> Are there laminate makers producing PTFE in Asia (other then Japan)?
I am not aware of PTFE laminate producers in Asia. The main suppliers of this material are:
Rogers, Taconic, Arlon, Metclad,...
> Are there PCB makers in Asia which can handle PTFE?
I know only one:
New Era Electronics Co, Ltd.
Taiwan
Tel: 886 3 4722191
Fax: 886 3 4723759
Email: [log in to unmask]
Of course, we can do it also. ;-)
I would be pleased to help you further.
Simon
Optiprint AG, Switzerland
http://www.optiprint.ch
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|