Hi Lou,
we are doing it on a quarterly basis for as long as I can remember and I
didn't notice any significant difference between each set of results. All
the contaminants are very low each time. And we passed all the ISO audits.
Frankly, I think that twice a year is not a bad idea.
Regards,
Ioan
> -----Original Message-----
> From: Lou Hart [SMTP:[log in to unmask]]
> Sent: Wednesday, July 11, 2001 9:54 AM
> To: [log in to unmask]
> Subject: [TN] Wave solder pot analysis
>
> TechNetters, I'd appreciate comments on contaminant analysis of a wave
> solder pot. We had been sending a sample out for analysis (type "C" I
> think it is, by the mil spec) once per month. Now the solder supplier is
> telling me that once every six months is more than enough. I've been
> taking the contaminant data and plotting Q charts (for short-run SPC the
> modern way, as I've been mentioning in this forum) with the monthly data.
> What has been your practice and recommendation?
>
> At the moment, it is hard for me to feel comfortable with a twice-yearly
> analysis of what seems to me to be an important material in our
> manufacturing process. Lou Hart
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|