Could you fellows enlighten me on toxicity of this additives please ,
and what goes into "standard" FR4 ?
Debate circulates about what harm can charring board do in a ventilator :
With or without retardant :
How far is the standard glass laminate prone to ignition/combustion/char and
what would be the effects of toxins generated ?
Thanks a lot
Paul Klasek
http://www.resmed.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################