Doug doing PB laminate speak? What's next; humor?
I have to agree with my esteemed colleague. Laminates that meet IPC-4101/26 or 29 would probably work in both those temperature ranges and it eliminates the need for polyimide.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, May 09, 2013 5:15 AM
To: [log in to unmask]
Subject: Re: [TN] Operating temperatures
A high quality FR4 with a Tg in the 175C range will work for #2, but I think you need polyimide to work up to 200C.
Doug Pauls
From: Pradeep Menon <[log in to unmask]>
To: <[log in to unmask]>
Date: 05/09/2013 06:09 AM
Subject: [TN] Operating temperatures
Sent by: TechNet <[log in to unmask]>
We have a requirement specified in the master drawing of couple of PCBs which indicate that the operating temperatures as below.
1. -50°C to 200°C operating PCB.
2. -40° to 150°C operating PCB.
Will a high Tg material FR4 meet this requirement. Or will Polyimide be required. Any general inputs on this since we could not find the operating temperature in the TDS of the materials
Rgds
Pradeep
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|