Yee, the water is pretty muddy our there with regard to surface finish
alternatives. One problem is, there seems to be an assumption that a
"one size fits all" product or process exists or will. I think this is
a mistake.
I always cringe when i read the ever popular "HASL" bashing posts, like
the recent one which portrays it as "gothic"?
The fact is, there are a lot of levels of packaging density out there.
HASL is a robust process with excellent solderability and sheflife when
done correctly. It may not be the correct choice on high density
designs.
Talking about surface finish alternatives without being specific about
application is well...more heat than light, eh?
Polling users without knowing there application can't be of much use.
Mark Simmons
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|