TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Tue, 18 Mar 2003 12:11:37 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Roger Stoops <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Roger Stoops <[log in to unmask]>
Parts/Attachments:
text/plain (56 lines)
Dow Corning 3145 (clear)
Been using it for years.
Any (true) equivalent would probably work just as well.  Do some testing with an unknown product first.
Also, James C. makes a good point, unless the instrument is not meant to be user-serviceable. Then again, you could ship a small tube of RTV with the product (chuckle, chuckle!).

And to answer Genny's first question:
     yes.

Roger



-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Tuesday, March 18, 2003 11:47 AM
To: [log in to unmask]
Subject: Re: [TN] How to hold component in socket


Genny

For goodness sake, do NOT use an RTV that smells of acetic acid. Wanna
know why? Because it emits acetic acid! And what does acetic acid do to
electronics, in a semi-closed environment and under uncontrolled
climatic conditions such as in transport? SHUDDER!

Brian

Genny Gibbard wrote:
> Do any of you seem to work somewhere where RTV is the answer to
> everything???
>
> We have a PCB with a DIMM socket.  The DIMM is inserted at one angle and
> then pushed down and 'locks' in at another angle to the PCB.  Problem
> is, the catch mechanism isn't very strong and sometimes the DIMM pops
> back up to the insertion angle.  We're concerned that when we ship these
> cards, the DIMM will pop loose and eventually work its way out of the
> socket.
> Any suggestions as to how to hold it in place?  We don't want to do it
> so permanently that we can't ever remove and replace a defective DIMM.
> The suggestion around here is a dab of silicone RTV...
>
> Genny
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2