TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Date:
Fri, 27 Jun 2008 14:13:32 -0700
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Happy Friday,

I need some help understanding how you test for the value of ceramic
capacitors. We build a board that has some 0603, .470 uF ceramic caps, +/-
10%. The assembly that these parts are on has been having a higher failure
rate at our ICT then we've seen in the past. We tracked the failure to this
cap which had a low reading. We replaced the cap and the unit passed ICT
just fine.

We measured the cap using our HP 4262A LCR Meter and sure enough it was
reading low, around .398 uF.

We pulled some new parts off the reel and they read low also ranging
anywhere from .398 to .425. We suspected that we had a bad reel of parts
even thought they were from a respected cap manufacturer.

Being curious we tested some more reels from different lot codes and found
the same thing. Being even more curious we tested some other parts from the
same manufacturer and found them to be low by around 5% - 7% and in some
cases slightly below 10%. We then tested some other parts from a different
manufacturer and they tested low also.

Now we are suspecting our test equipment so we went to an independent lab
and had them tested on an Andeen Hagerling 2500A Bridge. Guess what, we got
the same low readings.

After all that my question is, what are we doing wrong to get such low
readings on these ceramic caps? It just doesn't seem likely that four
different parts from three different major suppliers tested on two different
pieces of equipment would all be that far down on the low end.

Any education in capacitor testing and reading would surely be appreciated.

Best regards,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2