The Shadow Coating can have some issues with surface topography - we
have seen that as the batch ages the deposit thickness begins to vary
and the natural tooth of the shadow also is affected. I believe this
time we increased our system cleaning schedule (FSL Conveyorized) to
ensure buildup in sumps and rollers was minimized and also increased the
dump schedule of the bath.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: Mike Wolf [mailto:[log in to unmask]]
Sent: Tuesday, August 31, 2004 2:41 PM
To: [log in to unmask]
Subject: [TN] Resist adhesion failures
We are experiencing resist adhesion failures in a random spotty nature,
after develop traces and or pads will just not be adhered.
We run a cert. piece everyday that never has these problems. The cert
piece is ED/double treat right out of the box.
The copper that has the adhesion problems has been processed in our
shop, we run electrochem's shadow system.
I know its not much to go on more details available to anyone
interested.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|