TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Matthew Lamkin <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, Matthew Lamkin" <[log in to unmask]>
Date:
Fri, 14 Aug 1998 23:10:29 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Hi there,
You did not say how the solder got there in the first place ?
Perhaps the pads could be peelable masked to prevent solder adhering to them
during soldering.
just a thought...



-----Original Message-----
From: Steve Plant <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 11 August 1998 00:48
Subject: [TN] Solder on pads


Hi all,

Wondering if any of you could help me out.

We are currently assembling a product which requires us to bolt
busbars on top of PC boards into the IGBT's below the board. This
connection can pass up to 90 AMPs through it. Some of the
boards we are receiving have solder build-up on the pads and we
are spending some time clearing it off to provide us with a flat
surface.

My question is : Does anyone have any experience with this type
of sandwiching of PC boards and the effects of solder on the pads?

Is there any standards which we can use?

Any help would be most appreciated.


Regards


Steve Plant
Electronic Production Engineer.
PDL Electronics LTD.
New Zealand.
Ph (06) 843-5855       Fax (06) 843-5185
Email   [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2