TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 7 Jul 2008 15:34:35 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karl Hunsinger <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Karl Hunsinger <[log in to unmask]>
Parts/Attachments:
text/plain (51 lines)
Hi Graham,
	Hole sizes are typically finished hole size unless otherwise stated. IPC-2221 does not specify solder thickness. It does refer you to J-STD-006 for solderability testing. I'll send you a PDF of IPC-2221 offline.

Karl

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Collins
Sent: Monday, July 07, 2008 3:15 PM
To: [log in to unmask]
Subject: [TN] Flex specifications - tolerance on hole size


Hello TechNet
A question about through-holes on a flex.  We are having some debate about how to interpret a drawing.

Specifically, if I have a drawing that says:
1) fabricate per IPC 6013 type 4
2) tin-lead plating shall be per IPC 2221, method optional
3) hole size is specified in the drill schedule as 0.028", plated, +- 0.003"

Our debate is about the hole size after plating.  Does the +- 0.003" apply to the solder coated hole, or is that a copper only size?  Does IPC-2221 specify any maximum solder thickness?

I'm an assembler, so unfortunately I don't have these two IPC specs at hand.  

regards,
 
Graham Collins
Halifax Production Engineering
(902) 873-2000 ext. 6215


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2