TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 10 Feb 2012 15:42:04 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (46 lines)
Good afternoon all,

Recognizing that asking a question of this group late on a Friday 
afternoon is questionable judgement on my part, I will give it a shot 
anyway.

I am in the midst of the most perplexing material investigation of my 
life.  Provided I do not get shot, hung or tarred/feathered, I will have 
some neat stuff to publish in the next few years.  I have a general 
question on testing coatings, other than what you might do in aerospace.

Most temperature-humidity tests done on conformal coating are of the 
cyclical variety, 25C to 65C, 90% RH for a week.  This one is found in 
MIL-I-46058 and IPC-CC-830 and is used for material qualification. Nothing 
unusual there.

There are cyclical temperature-humidity test that are done as part of 
product qualification, such as DO-160E or MIL-STD-883.  But these are also 
of the cyclical variety and 25C to 65C is common there as well.  Nothing 
unusual there.

How would one simulate a coated assembly, stored in a cold and clammy 
environment (40-50F, 85-100% RH with probable dew points each day) for 
months at a time, then powered up?

Are there any tests done in your industry that tests a coatings resistance 
to a prolonged cold and clammy conditions?  Ideally with some form of 
acceleration factor?  I know that the automotive industry has something 
called a "damp heat" kind of test, but have no experience with that.

I know I can program my humidity chamber for an environment, but don't 
really have time to let it sit 3-6 months.  It has been suggested that I 
jump in my time machine and go back 6 months and I would be done by now, 
but my flux capacitor went through our Kyzen cleaning process and has no 
flux left.  I blame Hillman.

So, any thoughts would be appreciated. 

Doug Pauls


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2