Sounds like a crazy idea to me, 20 inch-pounds sounds like a heck of a lot.
I wonder what the bond strength between the copper and the laminate would
be. The land pattern make a fairly small surface area. Even if you don't rip
the component of the lands you might rip the lands off the board.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Carl Ray
> Sent: Wednesday, March 13, 2002 11:17 AM
> To: [log in to unmask]
> Subject: [TN] Solder Joint Mechanical Stress
>
>
> I have a customer who is requiring that I verify the bond strength of a
> heat sink that is glued to the top of PBGA. The customer has supplied me
> with a torque tool to verify the strength of the bond between the heat
> sink and the BGA. I have concerns that testing the strength of the glue
> bond may affect the solder joint reliability of the BGA. The tool
> supplied by the customer is set at 20 in pound torque. Any ideas how I
> can "change" my customer mind?
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|