TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wdEKB-000BjMC; Sun, 15 Jun 97 07:22 CDT
Old-Return-Path:
Date:
Sun, 15 Jun 1997 08:32:41 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Tue Jun 17 11:
17:53 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13419
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"gCUzF.0.9XL.2wzep"@ipc>
Subject:
From:
Status:
O
Message-ID:
X-Loop:
>From willli Sun Jun 15 07:
22:45 1997
Parts/Attachments:
text/plain (42 lines)
from running a few tin-nickels in the early 1980's at a few of my accounts -
i can give u some info on this process:

1-   sn/ni plating bath deposits an alloy with a 1:1 atomic ratio of tin to
nickel 
      or 65% tin and 35% nickel by weight

2-   excellent corrosion resistance, bright appearance and is extremely hard

3-   difficult or almost impossible to reflow - since it goes thru a metallic
phase change prior to melting

4-   it has a tendency to dull with age and forms a tenacious, chemically
resistant oxide on the surface which is self-healing

5-   high operating temperature - 140 - 160 F - increases resist leaching
into the plating bath

6-  poor deposit shelf life - due to the formation of the oxide film

u may want to conduct some tests prior to using this process in production - 

this data is provided on a process that was in use back in the 80's - someone
may have changed formaulation over the ages and maybe something new on the
market

regards

Richard Fudalewski
Atotech Canada Ltd

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2