Patranit

In answer to your questions:

1    No
2    No
3    J-STD 001A Appendix D

Sorry to be blunt. However, you might also refer to IPC 9201 SIR Test
Handbook.

Regards, Graham Naisbitt

[log in to unmask]

Concoat Ltd             Phone: +44 1276 691100
Alasan House          Fax:      +44 1276 691227
Albany Park
CAMBERLEY
GU15 2PL UK
-----Original Message-----
From: Patranit Waitayasuwan <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 25 March 1999 04:02
Subject: [TN] sir test


>Dear  Sir,
>Please  answer  my  question,
>The  purpose  of  SIR  test  :  - for   material  qualification
>                                - process  qualification
>1 Is  the  procedure  in  these  both  purpose  the  same?
>2. Is  the  test  coupon & test  condition of  these  the  same?
>3. What's   the  refernce  for process  qualification?
>
>Best  Regards,
>Patranit.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2