TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Thu, 17 Jul 2008 07:43:50 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (37 lines)
Hi Ioan,

Could you use a label like they put on boards, they go through all the
processes and stay on really good? Brady and other companies make them.

KennyB
-----Original Message-----
From: Ioan Tempea [mailto:[log in to unmask]] 
Sent: Thursday, July 17, 2008 7:35 AM
To: [log in to unmask]
Subject: [TN] Indelible marking

Dear Technos,

I need to serialize about 200 BGAs (simply write on them sequential
numbers 1-200). The BGAs will be assembled, SnPb process with water
soluble flux, then washed in plain water in our in-line washer.

In case the customer will not accept us scratching the numbers onto the
top of the components, what kind of permanent ink can I use?

And would you see any issue with scratching the top of the components?

Thanks,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2