TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Frank L Norman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 11 Sep 2003 09:48:22 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (127 lines)
Galvanic Series of Metals and Alloys in Sea Water
-------------------------------------------------

Positive Charge Anode(+)
Corroded end (anoxic, active, or least noble)

Magnesium Alloys
 Zinc
  Beryllium
   Cadmium
    Uranium
     Aluminum
      Indium
       Tin
        Stainless Steel 430
         Lead
          1010 Steel
           Cast Iron
            Stainless Steel 410
             Copper
              Nickel
               AM 350
                Chromium
                 Stainless Steel 350, 310, 304
                  Stainless Steel 430, 410
                   Stainless Steel 13-8, 17-7 PH
                    Brass, Yellow, Navel
                     Stainless Steel 316L
                      Bronze 220
                      Copper 110
                     Stainless Steel 347
                    Copper-Nickel 715
                   Stainless Steel 202
                  Monel 400
                 Stainless Steel 201
                Stainless Steel 321, 316
               Stainless Steel 309, 13-8, 17-7 PH
              Stainless Steel 304, 301, 321
             Stainless Steel 201, 316L
            Stainless Steel 286
           AM355
          Stainless Steel 202
         Carpenter 20
        AM355
       Titanium Alloys
      AM350
     Silver
    Palladium
   Gold
  Rhodium
 Platinum
Carbon/Graphite

Negative Charge Cathode(-)
Protected End (cathodic, passive, or more noble)


Regards,
Frank Norman
Manufacturing Support Engineer
Raytheon, Space and Airborne Systems (SAS)
(805)879-2745
[log in to unmask]





Steve Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/11/03 09:16 AM
Please respond to "TechNet E-Mail Forum."; Please respond to SteveZeva


        To:     [log in to unmask]
        cc:
        Subject:        Re: [TN] Zinc Plating Finish


Hi Victor!

What will probably happen is that the Zinc will start to corrode because
of the galvanic action between itself and the tin, or tin / lead. Go to:

http://www.ccfast.com/ccfcorrosion.html

There you will see a Galvanic Series chart, and a simple explaination
about Galvanic action. Zinc, and Tin or Tin / Lead isn't all that far
apart in the chart, but far enough that the Zinc will corrode.

-Steve Gregory-


Fellow TechNetters:

   What are the exposures of having or selecting a ZINC plating finish for
an ELECTRICAL CONTACT such as a solder less
crimp connector and straight pin connector.   What can occur if these
finishes are mixed mated with a SnPb or Sn finish surface.

Victor,



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2