You shouldn't have any problems at this level. Kester puts the limit at 0.3
citing MIL and J-STANDARDS. Klein-Wassink says anything below 0.2 is
perfectly fine. I'm puzzled about the 0.08 figure.
> -----Original Message-----
> From: Susan James [SMTP:[log in to unmask]]
> Sent: Wednesday, February 28, 2001 10:07 AM
> To: [log in to unmask]
> Subject: [TN] Copper levels in wave solder pot
>
> Gurus,
> After having our solder pot analyzed, the copper level is showing .1273.
> In July of 1999, the copper level was .120. We are assuming the copper is
> coming from the cut component leads. My concern is whether or not this is
> significant enough to change out the solder. J-STD-006 specs .08 as
> acceptable but I don't know how "bad" .1273 is considered to be. Any help
> is appreciated.
> Sue James
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|