TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Edwards <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Date:
Tue, 11 Sep 2012 13:50:01 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
I would be looking to see what operators are using to wipe down their stations and mats to make them oh so shiny...

Also check the actual wipers to see what has collected on them...

Paul

Paul Edwards
Process/Quality Engineering
Surface Art Engineering

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, September 11, 2012 9:10 AM
To: [log in to unmask]
Subject: [TN] Source of IC Contamination Species

Occasionally, IC analyses are reported to have elevated levels of acetates and formates.   Is it the general consensus that source of these contamination is assumed to be the decomposition of larger molecular weight weak organic acids found in soldering fluxes?  I can't imagine that any manufacturer would actually be placing acetic or formic acids directly into a flux formulation. These are much too volatile and aggressive. 

Thoughts?

Rich  Kraszewski 
Senior Process Engineer
PLEXUS 
 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2