TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 17 Apr 2007 07:18:50 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (84 lines)
However, I would caution anyone who wishes to try this: qualify it on your product first. I have no idea if it could cause problems in certain applications. 

-----Original Message-----
From: Stadem, Richard D. 
Sent: Tuesday, April 17, 2007 7:14 AM
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TN] Tacking corners of BGAs

Just a small amount capturing the corner on two sides. We had a requirement that none be touching the solderball itself. 

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, April 17, 2007 7:08 AM
To: [log in to unmask]; Stadem, Richard D.
Subject: RE: [TN] Tacking corners of BGAs

Can you share the Chip bonder application requirement for 4 corner BGA solder bump bonding?   ie: coverage - amount - height - etc.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, April 17, 2007 6:57 AM
To: [log in to unmask]
Subject: Re: [TN] Tacking corners of BGAs

I have used Chipbonder for many years to epoxy the four corners of BGAs. The reason I was doing this was to prevent any movement of the BGA during a second reflow. I did not want to go with full underfill as we wanted to be able to rework the BGAs in case of field failures. 
This method was first "tried out" on some scrap production boards, and it worked well using a solder paste designed to go through the reflow oven twice before wash (Kester R562). So my next step was to qualify the process, and I used two sets of assemblies, one set used the old method (no chipbonder) for benchmarking purposes. Qualification included running the assemblies through thermal cycling and microsectioning.
Imagine the surprise when the BGAs with the four corners bonded with a small bead of Chipbonder averaged 1610 cycles to failure compared to 967 for the ones without. The small amount of time required to bond the four corners was less than 30 seconds per BGA, manually.
Adding a little chipbonder in the four corners not only allowed us to gain our objective, but we greatly increased the reliability of the BGAs. 

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Monday, April 16, 2007 4:56 PM
To: [log in to unmask]
Subject: [TN] Tacking corners of BGAs

Dear Technetters,

 

We have a quality issue where some of our boards are returning because the BGAs need to be protected against mechanical stress.  We were considering using Loctite´s Chipbonder 348 on the corner of the BGAs in question (we would not to use an underfill).

 

Does anyone have any experience with Chipbonder 348 in this kind of application?

 

Would anyone care to suggest a heat-cured adhesive for tacking down corners of BGAs?

 

 

Thank you in advance,

 

David

[log in to unmask]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2