	Glenn: Amines and anhydrides are two general families of chemistry 
used as curing agents for epoxy resin systems. They help give the cured resin 
its particular properties and performance.	 			
	Dyanalloy Inc. makes a wide range of decapsulation and stripping 
formulations. You may want to try their DECAP or DYNASOLVE 185. These will 
breakdown both anhydride and amine systems.				
									
						Regards			
						Michael Barmuta		
						Staff Engineer		
						Fluke Electronics	
						Everett Wa.		
						425-356-6076		
						  
On Fri, 6 Jun 1997 12:46:44 -0700 [log in to unmask] wrote:

> From: [log in to unmask]> Date: Fri, 6 Jun 1997 12:46:44 -0700
> Subject: Fab/Assy: Decapsulant method
> To: [log in to unmask]
> 
> Technet,
> 	A while back there was a potential material listed that could remove 
> encapsulant.  The material is called URESOLVE PLUS from Dyanoloy.  Well, I 
> called the company and got some more information.  Not fully understanding 
all 
> the chemistry, they said it will work an epoxy with Anhydride based 
> activation, but not on Amine based.
> 	So, my question to you all, what is the chemical basis of 
> Photoresists, FR-4, GeTek(R), and Polyimide?  I'm not looking for trade 
> secrets, just info that should be the MSDS sheets.
> 
> Thanks very much for your help.
> 
> Glenn Pelkey
> Quality/Reliability Engineer
> Maxtek Components Corp.
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
> * with <subject: subscribe/unsubscribe> and no text in the body.          *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact   *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
> 



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2