TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 15 Jun 2007 03:22:54 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, N Burtt <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Parts/Attachments:
text/plain (22 lines)
OK it is Friday - and try as I might, can't resist picking on the typo for 
a "larger thermal ass"... I guess you just mean "big-a**ed" components?

But seriously with SnPb we found we got away with one profile for pretty 
much all shapes and sizes of PCBs. With lead-free we have found it important 
to trim the basic recipe to suit each and every design, making sure we profile 
a scrap board with a thermocouple on those parts we are concerned about 
(both thermally senstive =low max reflow temp/small thermal Mass and large 
thermal Mass)

Nigel

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2