TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 11 Mar 2003 11:01:24 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Zweigart, Siegmund" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Zweigart, Siegmund" <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
did you try vapor phase soldering

Siggi

-----Original Message-----
From: pohkh [mailto:[log in to unmask]]
Sent: Dienstag, 11. März 2003 10:57
To: [log in to unmask]
Subject: [TN] : rework or removal of SOT649A


Hi Technetters,

I happened to have boards with SOT649A, and I need to remove.

As this component is being soldered onto board which link to hugh ground
plane, I practically have no way to remove.

This component is easy to solder, but not for removing.

Is there anyone can advise me what can be done in order to get this SOT649A
component off the PCBA.

By the way, there is one piece of BGA on the opposite side of the PCBA.

Thanks.

Poh

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2