Hi Dale,
In all your descriptions, you are not telling us what the failure mode
actually is. On the basis of what do 75% not pass? Are the failures just some
undefined functional dysfuction?—your wire-bond inclusion in the discussion leads me
to believe this.
You also are not telling us what the reflow profiles [both standard and
increased] at the QFP leads [not the PCB soldering pads] are. This is needed to
make sure that the heat sink, which the die is and to which the leads are
attached, does not keep the lead temperature too low even with your increased
profile.
Werner Engelmaier
Future workshops:
Solder Joint Reliability: Parts 1 through 4, July 21/22, Hamburg, Germany
Pb-Free Soldering Processes—Survival, Quality, Reliability, August 18,
Orlando
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture,
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
Solder Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania
Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
**************
Get fantasy football with free live scoring. Sign up for
FanHouse Fantasy Football today.
(http://www.fanhouse.com/fantasyaffair?ncid=aolspr00050000000020)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|