TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vDYle-0000UEC; Wed, 16 Oct 96 11:24 CDT
Old-Return-Path:
Date:
Wed, 16 Oct 96 08:57:04 EST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/6921
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"dH2PZ3.0.sV7.omGPo"@ipc>
Subject:
From:
"Hollandsworth, Ron" <[log in to unmask]>
From [log in to unmask] Wed Oct 16 12:
06:40 1996
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (19 lines)
     Years ago I attended Ralph Woodgates "Zero Defects Soldering 
     Seminar" in which he stated that rework/touchup on solder 
     joints can degrade them.  He also stated that solder joints 
     that have been reworked are inclined to fail before joints 
     that have not been reworked.  You may want to contact Ralph 
     Woodgate for more detail on tests run in the past.  His 
     offices were in New York.  I am not sure of his number or 
     fax.  There are probably some TechNetter who still have his 
     number.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2