text/plain (21 lines)
We've observed what could be described as 'whisker's' on one lot some
time ago...after evaluation we determined it to be caused by inadequate
cleaning prior to the immersion bath. We really are not concerned about
whiskers.

A big difference is in the grain structure which is very uniform and
closely bonded in comparison to 'plain old tin' plating which has a
loose, course grain structure...what this leads to is a flat surface
that does not attract or retain contaminates like the 'old' tin baths...

Franklin

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2