As long as you apply current (recommended for application Current Density) and tin solution within spec it will plate. So it is not self limited.
Regards
Aleks Lozinsky
Technical Sales Representative
Technic Canada
195 Riviera Drive
Markham, Ontario
Canada
L3R5J6
001+905 940 4020 Office
001+416 450 1093 mobile
[log in to unmask]
http://www.technic.com
This e-mail is confidential. Any unauthorized disclosure, use or dissemination, either whole or partial, is prohibited. If you are not the intended recipient of the message, please notify the sender immediately.
-----Original Message-----
From: Victor Hernandez <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 17 Jul 2013 08:49:46
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
<[log in to unmask]>
Subject: [TN] Bright tin Plating, electrolytic plating
Fellow TechNetters:
Is electrolytic bright tin plating self-limiting in thickness?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|