     Ron,
     Enthone.OMI is the company that markets an OSP process by the trade 
     name of Entek.
     
     Their Calif. office is located at 2779 El Presidio St. in Long Beach.
     Phone # 310.537.0288, Fax# 310.637.2595
     
     
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Entech
Author:  [log in to unmask] at internet
Date:    8/6/96 1:04 PM


One of our students is looking for information on the Entech coating process 
for copper lines. Can anyone tell me where to find that? I have heard of it 
as a process ... is it a company as well? 
Ron Gedney
[log in to unmask]
Integrated Electronic Eng. Center
Watson School of Eng. & Applied Science 
Binghamton University
P.O. Box 6000
Binghamton, NY 13902
607-777-4335, fax 4683
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2