Hi Jim,
In my limited experience with solder joint requirements, the "j" hook is
required when soldering in accordance with the weapons specification
(WS-????), however, I'm not familiar with an IPC req't. The obvious
advantage of using a "j" hook is based on additional support of the joint
when the joint may experience mechanical stress in the field.
Hope this helps...
Frank Freitas
------Original Message------
From: "West, Jim" <[log in to unmask]>
To: [log in to unmask]
Sent: December 3, 1999 3:35:25 PM GMT
Subject: [TN] Soldering with J-hook
Hi everyone,
I was looking through the IPC book and I may be overlooking this, but is
there a requirement that says
you must use a J-hook technique when soldering two discrete wires together
or soldering a discrete wire
to a potentiometer lead? I believe that creating a good mechanical
connection is priority #1 and then
solder the joint. But, is it ok to just lay the two wire ends on top of
each other and solder the joint and same
with the potentiometer, is it ok to lay the discrete wire on the
potentiometers lead and then solder the joint.
If anyone can give me some pro's and con's to both techniques, I would
greatly appreciate it.
Jim
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
-----------------------------------------------
FREE! The World's Best Email Address @email.com
Reserve your name now at http://www.email.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|