"Valerie St.Cyr" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 18 Nov 2004 13:02:17 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (100 lines)
ditto... that's what I use; "array" being preferred; "assembly panel"
second.





Dwight Mattix <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/18/2004 12:12 PM
Please respond to TechNet E-Mail Forum; Please respond to Dwight Mattix


        To:     [log in to unmask]
        cc:
        Subject:        Re: [TN] English expression


Alternately, and I'd argue more precisely you can describe it as an
"array"
or an "assembly panel."

As noted by others "panel" is the most commonly used term.  However,
sometimes it gets confusing when talking with our PWB supplier since they
use the term panel for their fab panel.

I prefer to describe our assembly panel as an "array" so as to distinguish
between our "assembly panel" and the PWB fabricator's (much larger) "fab
panel."

...a fine point not worth quibbling about but that's my $0.02.

cheers,
Dwight


At 08:19 AM 11/18/2004, you wrote:
>Hi all
>When small PCBs are assembled and soldered they are together in a
>larger unit and separated after the production.
>Whats the English expression of this unit. In German we call that
>"Nutzen" (that's for Werner it might help him to understand what I
>mean).
>
>Thanks a lot for your help
>
>Guenter
>
>EMPA
>Swiss Federal Laboratories  for Materials Testing and Research
>Centre for Reliability
>Guenter Grossmann,  Senior Engineer
>
>8600 Duebendorf
>Switzerland
>
>Phone: xx41 1 823 4279
>Fax :     xx41 1 823 4054
>mail:     [log in to unmask]
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2