Hi Richard,
I'm not sure if you found your answer yet. Clause 6.1 of the J-Std-001 Revision E states "Components that are required to be mounted off the board, shall be elevated at least 1.5 mm [0.059 in.]".
It doesn't specifically use the term "power resistor" but it is usually a higher watt resistor that receives this type of treatment.
I hope this helps.
Best Regards,
Jeff
Jeff Popp - QA Technician
Compunetix, Inc.
2420 Mosside Blvd.
Monroeville, PA 15146
(412) 858-6184
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: Wednesday, July 27, 2011 12:38 PM
To: [log in to unmask]
Subject: [TN] Requirement to PTH Mount Power Resistors Above PWB Surface
Where is the requirement for power resistors to be installed above the PWB surface? I thought it was in J-STD-001, but I can't find it.
Dick Krug, SSBB, CSMTPE
SMT Process Engineer
Sparton Corporation
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|