TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0u7Sgx-0000AYC; Thu, 11 Apr 96 15:10 CDT
Encoding:
7 TEXT
Old-Return-Path:
Date:
Thu, 11 Apr 96 15:17:00 PDT
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
From [log in to unmask] Thu Apr 11 16:
12:34 1996
TO:
IPC Technet <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"UrlBk2.0.nWF.USMRn"@ipc>
Subject:
From:
Kaylor Karl <[log in to unmask]>
X-Loop:
X-Mailing-List:
<[log in to unmask]> archive/latest/3401
X-Mailer:
Microsoft Mail V3.0
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (10 lines)

We are having a problem with melf diode components being open after reflow 
solder.  Would using the IPC detent pattern reduce this problem?